Patentes CM
Logo

NI-MN LDH ELECTRODES FOR ORGANIC POLLUTANT DEGRADATION IN WASTEWATER

Universitat de València

Detalles de la patente

Resumen

The present invention relates to the field of water treatment technologies, specifically to the development of electrochemical electrodes for the removal and degradation of organic pollutants from water. The invention particularly focuses on the use of nickel-manganese layered double hydroxide (NiMn-LDH) electrodes, modified with various carbon materials and supported on a graphite felt substrate, to enhance the efficiency and effectiveness of electrochemical oxidation processes in water purification.

Reivindicaciones

  1. An electrocatalytic material characterized in that it comprises • a conductive carbon material as a support; • a nickel-manganese layered double hydroxide deposited homogeneously over the support; wherein the amount of conductive carbon material is between 10% and 15% in weight with respect to the nickel-manganese layered double hydroxide; and wherein the ratio of nickel with respect the manganese in the layered double hydroxide is between 2.5:1 and 4:1, preferably 2.8:1 and 3.2:1.
  2. Electrocatalytic material according to claim 1, wherein the conductive carbon material is selected from carbon nanotubes, graphene, reduced graphene oxide, carbon black, activated carbon, carbon fibers, carbon nanonions, carbon dots, mesoporous carbon, and carbon nanotubes with carboxylmethyl cellulose.
  3. Electrocatalytic material according to claim 2, wherein the conductive carbon material is carbon nanotubes.
  4. A process to obtain the electrocatalytic material described in any claims 1 to 3, characterized in that it comprises the following steps: a) mixing a conductive carbon material with a 1.2 w/V% to 6 w/V% of H<2>O<2> 30% solution; b) oxidizing the mixture obtained in step (a), filtering and drying the oxidized conductive carbon material obtained; c) mixing in a solution of methanol, preferably dry methanol, the metal precursors of Ni and Mn in a stoichiometric ratio of between 2.5:1 and 4:1 respect to Ni:Mn and then adding the oxidized conductive carbon material obtained in step (b) wherein the ratio of oxidized conductive carbon material is between 6:1 and 8:1 with respect to the nickel-manganese; d) preparing a NaOH solution in methanol with a concentration ranging from 0.1 M to 6 M and adding it slowly to the mixture, preferably by dropwise technique, obtained in step (c) over a period of 2 to 100 minutes, followed by stirring the mixture for a minimum of 48 hours and the obtained dispersion is filtering; and e) drying the powder obtained in step (d), preferably in a temperature of between 15 °C and 80 °C.
  5. Process according to claim 4, wherein the conductive carbon material is selected from carbon nanotubes, graphene, reduced graphene oxide, carbon black, activated carbon, carbon fibers, carbon nano-onions, carbon dots mesoporous carbon, and carbon nanotubes with carboxymethyl cellulose, preferably the conductive carbon material is carbon nanotubes.
  6. Process according to any of claims 4 or 5, wherein the oxidizing of step (b) is a treatment using a microwave furnace at 450 W during 6 minutes.
  7. Process according to any claims 4 to 6, wherein the metal precursors of step (c) are Ni and Mn is in a stoichiometric ratio of between 2.8:1 and 3.2:1, preferably the precursor are halide salts, nitrate salts, sulfate salts.
  8. Process according to any claims 4 to 7, wherein the ratio of oxidized conductive carbon material with respect to the nickel-manganese and the ratio of nickel-manganese is between 1:6.8 and 1:7.8.
  9. An electrocatalytic device characterized in that it comprises: • an electrocatalytic material according to any of claims 1 to 3 deposited on a graphite felt configured to act as an anode or negative electrode.
  10. Process for obtainment of an electrocatalytic material deposited on a graphite felt described in claim 9 characterized in that it comprises the following steps: i. cleaning a graphite felt; ii. increasing the surface tension of the cleaned graphite felt obtained in step (i); iii. oxidizing the graphite felt obtained in step (ii); iv. impregnating the oxidated graphite felt obtained in step (iii), with the metal salts precursors of Ni and Mn in a stoichiometric ratio of between 2.5:1 and 4:1, preferably metal salt precursors are selected from halide salts, nitrate salts, sulfate salts, and optionally further adding a conductive carbon material; v. adding the precipitating agent to the mixture obtained in step (iv) in an amount of at least 2 times the stoichiometric amount of the metals present in the mixture, preferably the precipitation agent is selected from NaOH and Glycidol; vi. rinsing of excess powder obtained in step (v) with at least twice a volume of polar solvent, preferably water, with respect to the total volume obtained in step (v) and drying, preferably in a temperature of between 15 °C and 80 °C.
  11. Process according to claim 10, wherein the cleaning of step (i) is carried out by washing with a polar solvent selected from methanol or acetone.
  12. Process according to any of claims 10 or 11, wherein increasing the surface tension of step (ii) is carried out by a corona treatment.
  13. Process according to any of claims 10 to 12, wherein the oxidizing of step (iii) is carried out by immersing in H<2>O<2> and irradiating for 3-6 minutes at 450W in a microwave.
  14. Use of the electrocatalytic material described in any claims 1 to 3 or the electrode described in claim 9, as an anode in an electrochemical oxidation process of wastewater for the removal and degradation of their organic pollutants, preferably the organic pollutant is phenol.
  15. Method for wastewater treatment characterized in that it comprises the following steps: 1) contacting the electrochemical device described in claim 9, in a medium comprising waste water; 2) applying a current density of between 5 and 20 mA·cm<2>; 3) sampling of the water to be treated for intervals between 2.5 and 20 min; 4) analyzing the evolution of the samples of step (3) of the phenol concentration and the chemical oxygen demand (COD); and 5) optionally cleaning by keeping the device and the anode immersed in milliQ water for at least 1 h.
Inventores
  • Mirehbar, Seyedkeyvan
  • Seijas da Silva, Alvaro
  • Jaramillo Hernández, Camilo Andrés
  • Lado Garrido, Julio J
  • Abellán Sáez, Gonzalo
  • Palma del Val, Francisco Jesús
Solicitantes
  • Universitat de València
  • Fundación IMDEA Energía
  • Matteco Team S.L.
Clasificación IPC

C02F 1/ 461 A I, C02F 1/ 467 A I, C25B 11/ 02 A I, C25B 11/ 065 A I, C25B 11/ 091 A I

Nº de publicación

EP.4778892.A1

Fecha de publicación

22 de julio de 2026

Nº de solicitud

25382024

Fecha de presentación

17 de enero de 2025

Estado legal
docdbfechacodigodescripcion
EP.4778892.A12026-07-22AKDESIGNATED CONTRACTING STATES
EP.4778892.A12026-06-19PUAIPUBLIC REFERENCE MADE UNDER ARTICLE 153(3) EPC TO A PUBLISHED INTERNATIONAL APPLICATION THAT HAS ENTERED THE EUROPEAN PHASE
EP.4778892.A12026-06-19STAAINFORMATION ON THE STATUS OF AN EP PATENT APPLICATION OR GRANTED EP PATENT
Patentes relacionadas