Patentes CM
Logo

Method for preparing transparent and conducting sheets on polymers

Centro de Investigaciones Energéticas, Medioambientales y Tecnológicas

Detalles de la patente

Resumen

A method is proposed for preparing transparent and conducting sheets on polymers. A vertical structure is formed stacked on a polymer base depositing a transparent coating of indium oxide doped with tin (ITO) to provide a suitable substrate for optoelectronic applications. The ITO electrode has a preferential crystalline orientation on the plane (111). The formation of this film improves the physical properties of the substrate, reaching a high transparency value, an average of close to 80% in the 400-1100 nm spectra range, and conductivity, sigma > 10<3> ( OMEGA xcm)<-1>. The ITO films manufactured by the method proposed do not require heating of the substrate during the preparation of the layer, or treatment after deposition, to obtain high optoelectronic quality. The use of a pre-treatment with plasma of the organic sheets lead to obtaining adherent films without damaging the polymer sheets. <IMAGE>

Reivindicaciones

  1. Method for preparing transparent and conducting sheets on polymers used as substrates for optoelectronic applications, consisting of a base polymer to deposit a thin film coating, substantially conducting and transparent, of indium oxide electrode doped with tin (ITO) applied to the surface of the polymer, on which electric contacts can be joined to said ITO layer to receive a polarisation voltage and/or extract electric current, characterised in that it consists of the following stages; conditioning polymer sheets; treating the polymer surface with nitrogen plasma; depositing said ITO electrodes by cathode sputtering; and, if required, vacuum evaporating the superior electric contacts.
  2. Method according to claim 1, characterised in that said polymer sheets are polyethylene terephtalate (polyester or PET), and polyimide (Kapton KJ® ).
  3. Method according to claim 1, characterised in that said treatment of the substrate with nitrogen plasma consists of the following steps: placing said polymer substrates in a substrate holder in a vacuum chamber at 1x10<-4> Pa or less; connecting said substrate holder to a source of supply; establishing a nitrogen gas flow in said vacuum chamber, maintaining the pressure in the vacuum chamber at 2 Pa; establishing the power level for the ignition of the plasma in order to start the plasma attack on the exposed side of said polymer substrates; reducing the power level until the plasma is extinguished after the time required for the preparation of said exposed side of the polymer substrate.
  4. Method according to claim 1, characterised in that the time established for said plasma attack on the substrate is approximately 20 seconds.
  5. Method according to claim 1, characterised in that said deposition by cathode sputtering of said ITO electrodes consists of the following stages: leaving said substrates in the vacuum chamber in the substrate holder, again reducing the vacuum pressure to 1x10<-4> Pa; positioning a cathode sputtering target over said substrate holder; connecting the sputtering target to the source of supply; establishing a flow of argon and oxygen gases inside the vacuum chamber, forming a reactive argon/oxygen atmosphere; maintaining the pressure in the vacuum chamber at 0.5 Pa; establishing the power level; igniting a plasma to start the cathode sputtering of the material of the target on the exposed side of the polymer substrates; reducing the power level until the plasma is extinguished after obtaining the thickness required for the ITO electrode on the polymer substrates.
  6. Method according to claim 1, characterised in that the cathode sputtering target consists of a mix of indium oxides and tin in tablet form.
  7. Method according to claim 1, characterised in that the mix of indium oxides and tin is formed by In<2> O<3> /SnO<2> in a ratio of 19/1.
  8. Method according to claim 1, characterised in that the cathode sputtering process is established with a deposition speed of 1.2 nm/s for the ITO electrode.
  9. Method according to claim 1, characterised in that the ITO electrode is prepared without heating the polymer sheets of claim 3.
  10. Method according to claim 1, characterised in that the ITO film is prepared in reactive sputtering conditions, without damaging the polymer sheets of claim 2 in the reactive argon/oxygen atmosphere used.
  11. Method according to claim 1, characterised in that the substrate has a light transmission of nearly 80 % in the 400-1100 nm spectra range.
  12. Method according to claim 1, characterised in that the ITO electrode analysed by X-ray diffraction shows an intensity ratio of the principal (400)/(222) peaks of up to 0.83.
  13. Method according to claim 1, characterised in that the ITO electrode on a polymer sheet base has a resistivity value as low as 4 Ω/square.
Inventores
  • Herrero Rueda, Jose
  • Guillen Arqueros, Cecilia
Solicitantes
  • Centro de Investigaciones Energéticas, Medioambientales y Tecnológicas
Clasificación IPC

G02F 1/ 1343 A I, H01B 1/ 08 A I, H01L 31/ 18 A I

Nº de publicación

EP.1367653.A1

Fecha de publicación

3 de diciembre de 2003

Nº de solicitud

02380111

Fecha de presentación

27 de mayo de 2002

Estado legal
docdbfechacodigodescripcion
EP.1367653.A12011-06-2918DAPPLICATION DEEMED TO BE WITHDRAWN
EP.1367653.A12011-05-27STAAINFORMATION ON THE STATUS OF AN EP PATENT APPLICATION OR GRANTED EP PATENT
EP.1367653.A12008-10-2217QFIRST EXAMINATION REPORT DESPATCHED
EP.1367653.A12004-08-25AKXDESIGNATION FEES PAID
EP.1367653.A12004-07-2817PREQUEST FOR EXAMINATION FILED
EP.1367653.A12003-12-03AKDESIGNATED CONTRACTING STATES
EP.1367653.A12003-12-03AXREQUEST FOR EXTENSION OF THE EUROPEAN PATENT
EP.1367653.A12003-10-17PUAIPUBLIC REFERENCE MADE UNDER ARTICLE 153(3) EPC TO A PUBLISHED INTERNATIONAL APPLICATION THAT HAS ENTERED THE EUROPEAN PHASE
Patentes relacionadas