The method involves treating residue liquid to destabilize the emulsion of oils or fats and decantation to obtain a light phase with oils or fats and a heavy phase. A chloride electrolyte, carbonate and an alkaline metal hydroxide or an alkaline metal is added to the heavy phase and given heat treatment at a temperature of 50-80[deg] C. The light phase is decanted to obtain polyalkyl glycol with heavy phase which is purified and separated to obtain glycols and the electrolytes.
C02F 9/ 10 A I
ES.2300189.A1
1 de junio de 2008
200601389
26 de mayo de 2006
| docdb | fecha | codigo | descripcion |
|---|---|---|---|
| ES.2300189.A1 | 2026-06-02 | FD2A | ANNOUNCEMENT OF LAPSE IN SPAIN |
| ES.2300189.A1 | 2009-06-08 | FG2A | DEFINITIVE PROTECTION |
| ES.2300189.A1 | 2008-06-01 | EC2A | SEARCH REPORT PUBLISHED |