The method involves extracting the profiles from zinc, aluminum and silver alloys. The profiles are of simple or complex symmetry. The content of the base elements of the alloy ranges between 20 to 23 percent by weight in case of aluminum, 0.5 to 4 percent by weight of silver a remaining weight as zinc. The manufacturing method involves preheating ingot, where extrusion and cooling of the profiles is carried out at room temperature.
B21C 23/ 00 A I, C22C 18/ 04 A I
ES.2288097.A1
16 de diciembre de 2007
ES20050002766
11 de noviembre de 2005
| docdb | fecha | codigo | descripcion |
|---|---|---|---|
| ES.2288097.A1 | 2025-11-26 | FD2A | ANNOUNCEMENT OF LAPSE IN SPAIN |
| ES.2288097.A1 | 2009-04-01 | FG2A | DEFINITIVE PROTECTION |
| ES.2288097.A1 | 2007-12-16 | EC2A | SEARCH REPORT PUBLISHED |