Resumen

[0001] The invention consists of depositing tin-doped indium oxide and aluminium-doped zinc oxide on glass substrates without intentional heating, by means of the sputtering technique. It consists of the following stages: In order to prepare them, substrates are degreased and cleansed in an ultrasonic bath, rinsed in deionised water and dried with air jet. The substrates to be coated are then placed in a sputtering chamber and bombarded with Ar+ ions. Indium oxide or zinc oxide target surfaces are prepared by bombarding them with Ar+ ions. The substrates are coated with the material which makes up the targets, whilst a flux of argon and oxygen is maintained in the sputtering chamber. The oxygen flux should preferably be between 0.5 and 1sccm. The radiofrequency power density throughout this procedure is between 4000 and 10000 mW/cm2. This process allows us to obtain thin films of both materials with high electrical conductivity and high transparency to visible light.

Reivindicaciones

  1. Method for obtaining electrical and transparent conducting oxides by means of cathode grinding without substrate heating, characterised in that it comprises the following stages: - the preparation of the substrates by degreasing them with organic solvents and cleansing them in an ultrasonic bath with neutral water and soap, after which they are rinsed with deionised water and finally dried with an air pistol; - the introduction of the substrates that are to be coated with transparent conducting oxides in a cathode grinding chamber, where they are bombarded with Ar<+> ions; - the preparation of indium oxide or zinc oxide target surfaces by bombarding them with Ar<+> ions. - the coating of the substrates with the materials which make up the targets, whilst a flux of argon and oxygen is maintained in the cathode grinding chamber.
  2. Method for obtaining electrical and transparent conducting oxides by means of cathode grinding without substrate heating, according to claim 1, characterised in that the targets are made up of In2O3:SnO2 (95/5% in weight) and ZnO:Al2O3 (98/2% in weight), the argon flux is comprised between 0 and 150 sccm and the oxygen flux is comprised between 0.5 and 1 sccm and the radiofrequency power density between 4000 and 10000mW/cm2.
Inventores
  • Martinez Calvo, Maria Angeles
  • Gutierrez Garcia, Maria Teresa
  • Herrero Rueda, Jose
Solicitantes
  • Centro de Investigaciones Energéticas, Medioambientales y Tecnológicas
Clasificación IPC

C03C 17/ 245 A I, C23C 14/ 08 A I

Nº de publicación

EP.1184481.A2

Fecha de publicación

6 de marzo de 2002

Nº de solicitud

01500202

Fecha de presentación

27 de julio de 2001

Estado legal
docdbfechacodigodescripcion
EP.1184481.A22007-08-0118DAPPLICATION DEEMED TO BE WITHDRAWN
EP.1184481.A22007-06-29STAAINFORMATION ON THE STATUS OF AN EP PATENT APPLICATION OR GRANTED EP PATENT
EP.1184481.A22004-08-25AKXDESIGNATION FEES PAID
EP.1184481.A22004-07-2817PREQUEST FOR EXAMINATION FILED
EP.1184481.A22003-12-03AKDESIGNATED CONTRACTING STATES
EP.1184481.A22003-12-03AXREQUEST FOR EXTENSION OF THE EUROPEAN PATENT
EP.1184481.A22003-12-03RIC1INFORMATION PROVIDED ON IPC CODE ASSIGNED BEFORE GRANT
EP.1184481.A22003-12-03RIC1INFORMATION PROVIDED ON IPC CODE ASSIGNED BEFORE GRANT
EP.1184481.A22003-12-03RIC1INFORMATION PROVIDED ON IPC CODE ASSIGNED BEFORE GRANT
EP.1184481.A22003-12-03RIC1INFORMATION PROVIDED ON IPC CODE ASSIGNED BEFORE GRANT
EP.1184481.A22003-10-17PUALSEARCH REPORT DESPATCHED
EP.1184481.A22002-03-06AKDESIGNATED CONTRACTING STATES
EP.1184481.A22002-03-06AXREQUEST FOR EXTENSION OF THE EUROPEAN PATENT
EP.1184481.A22002-01-18PUAIPUBLIC REFERENCE MADE UNDER ARTICLE 153(3) EPC TO A PUBLISHED INTERNATIONAL APPLICATION THAT HAS ENTERED THE EUROPEAN PHASE
Patentes relacionadas