Process for the preparation of two-dimensional V 2 O[sub,3}, material thus obtained and use thereof. The present invention relates to a direct and low-cost process for obtaining two-dimensional V 2 O 3 of nanometric size comprising the following steps: a) grinding pristine microcrystalline V 2 O 5 powders , b) preparing a solution of NaF in ethanol and dispersing the V 2 O 5 ground in the previous step, c) heating the solution prepared with the V 2 O 5 dispersed in step b) to a temperature between 200 and 250°C for a time between 20 and 30 h in a closed reactor, thus obtaining V 2 O 3 nanosheets and d) collecting the V 2 O 3 nanosheets obtained in step c) and washing them with distilled water and ethanol. The invention also relates to the oxide thus obtained and its use as an anodic material in lithium ion (Li-ion) batteries. (Machine-translation by Google Translate, not legally binding)
C01G 31/ 02 A I, H01M 4/ 139 A I
ES.2982864.A1
17 de octubre de 2024
202330220
16 de marzo de 2023
| docdb | fecha | codigo | descripcion |
|---|---|---|---|
| ES.2982864.A1 | 2026-10-05 | PC2A | TRANSFER OF PATENT |
| ES.2982864.A1 | 2024-10-17 | BA2A | PATENT APPLICATION PUBLISHED |