The coating of metal components preventing oxidation by high-temperature steam consists of application of liquid containing aluminium and e.g. nickel in a powder (20-60):(40-80) weight ratio. This suspension is then treated successively at 60-100, 250-400 and 625-900 degrees C for 1-20,20-50 and 60-900 minutes respectively, on a repetitive basis. The metal component, e.g. a 20 per cent chromium steel steam turbine part, is coated with e.g. phosphate-based solution also containing silicon, at less than 20 per cent of the 3-10 micron powder mix.
C09D 5/ 10 A I, C23C 20/ 04 A I
ES.2251876.A1
1 de mayo de 2006
200402547
25 de octubre de 2004
| docdb | fecha | codigo | descripcion |
|---|---|---|---|
| ES.2251876.A1 | 2018-10-08 | FD2A | ANNOUNCEMENT OF LAPSE IN SPAIN |
| ES.2251876.A1 | 2007-07-01 | FG2A | DEFINITIVE PROTECTION |
| ES.2251876.A1 | 2006-05-01 | EC2A | SEARCH REPORT PUBLISHED |