A method for stabilizing phosphogypsum, characterized in that it comprises the following steps: a) initial preparation of the phosphogypsum by means of filtration, neutralization to a pH of at least 4, and drying to a moisture content of at most 10%; b) preparation of a mixture of at least gravel, sand, elemental sulphur and the phosphogypsum resulting from step a); c) heating of said mixture resulting from step b) between 150°C and 165°C; d) cooling of the mixture obtained in step c) to 130-150°C and addition of at least one sulphur polymer, resulting in a polymeric sulphur cement; e) forming, by means of vibration, of the polymeric cement obtained in step d); and f) cooling of the formed polymeric cement.
C04B 11/ 26 A I, C04B 18/ 04 A I, C04B 28/ 14 A I
C04B22/144, C04B24/16, C04B28/143, C04B28/36
WO.2012127090.A1
27 de septiembre de 2012
2012070178
21 de marzo de 2012
| docdb | fecha | codigo | descripcion |
|---|---|---|---|
| WO.2012127090.A1 | 2014-04-16 | 122 | EP: PCT APPLICATION NON-ENTRY IN EUROPEAN PHASE |
| WO.2012127090.A1 | 2013-09-23 | NENP | NON-ENTRY INTO THE NATIONAL PHASE |
| WO.2012127090.A1 | 2012-11-14 | 121 | EP: THE EPO HAS BEEN INFORMED BY WIPO THAT EP WAS DESIGNATED IN THIS APPLICATION |