FERRITE TYPE MATERIALS AND PROCESS FOR THE PRODUCTION THEREOF

Institutt for Energiteknikk

Detalles de la patente

Resumen

A process for producing a two-phase ferrite powder comprising: a) Sr-ferrite as a first phase; b) an iron oxide as a second phase, wherein said process comprises the steps of v) milling a Sr-ferrite starting material for a duration of 10 min to 6 hours; and vi) heating the material obtained in step i) to a temperature of 500-2000 °C.

Reivindicaciones

  1. Claims 1 . A process for producing a two-phase ferrite powder comprising a) Sr-ferrite as a first phase b) an iron oxide as a second phase, wherein said process comprises the steps of i) milling a Sr-ferrite starting material for a duration of 10 min to 6 hours; and ii) heating the material obtained in step i) to a temperature of 500-2000 °C.
  2. The process as claimed in claim 1 , wherein the milling in step i) is carried out for a duration of 15 min to 4 hours, preferably 20 min to 2 hours, more preferably 20 min to 1 hour.
  3. The process as claimed in claim 1 , wherein the milling in step i) is carried out for a duration of 10 min to 1 hour.
  4. The process as claimed in any preceding claim, wherein the two-phase ferrite powder has a coercivity of greater than 4.5 kOe.
  5. The process as claimed in any preceding claim, wherein the particles obtained in step i) have an average size of less than 1 μηη in the longest direction, preferably less than 750 nm, more preferably less than 500 nm in the longest direction, such as in the range 50-1000 nm, preferably 100-750 nm.
  6. The process as claimed in any preceding claim, wherein the Sr-ferrite starting material is selected from a low grade Sr-ferrite, high grade Sr-ferrite and recycled Sr-ferrite, or blends of two or more thereof.
  7. The process as claimed in any preceding claim, wherein iron oxide is produced in step i) in an amount of 0.1 -15 wt%, preferably 0.5-10 wt%, preferably 1 -8 wt%, preferably 3-7 wt%, based on the total weight of the powder obtained in step i).
  8. The process as claimed in any preceding claim, wherein in step ii) the heating is carried out at a temperature of 500-1500 °C, preferably 800-1200 °C, more preferably 900-1 100 °C.
  9. The process as claimed in any preceding claim, wherein in step ii) the heating is carried out for 15 min - 4 hours, such as 30 min - 2 hours, e.g.
  10. hour.
  11. The process as claimed in any preceding claim, wherein the iron oxide is Fe<2>0<3>.
  12. 1 . The process as claimed in any preceding claim, wherein the milling in step i) is performed with less than 1 wt% processing control agent (PCA) such as liquid PCA (e.g. water and/or toluene) or solid PCA (stearic acid); preferably the milling in step i) is performed in the absence of a processing control agent (PCA) such as liquid PCA (e.g. water and/or toluene) or solid PCA (stearic acid).
  13. The process as claimed in any preceding claim, wherein the material milled in step i) comprises at least 90 wt% Sr-ferrite starting material, e.g. at least 95 wt%, 99 wt% or 99.9 wt% Sr-ferrite starting material.
  14. A process for producing a two-phase ferrite powder comprising a) Sr-ferrite as a first phase b) an iron oxide as a second phase, wherein said process comprises the steps of: iii) milling a mixture of a Sr-ferrite starting material and iron oxide for a duration of 10 min to 6 hours; and iv) heating the material obtained in step iii) to a temperature of 500-2000 14. The process as claimed in claim 13, wherein the milling in step iii) is carried out for a duration of 15 min to 4 hours, preferably 15 min to 2 hours, more preferably 15 min to 1 hour, such as 15 min to 45 min, or 15 min to 35 min.
  15. The process as claimed in claim 13, wherein the milling in step iii) is carried out for a duration of 10 min to 1 hour.
  16. The process as claimed in any of claims 13-15, wherein the two-phase ferrite powder has a coercivity of greater than 4.5 kOe.
  17. The process as claimed in any of claims 13 to 16, wherein the particles obtained in step iii) have an average size of less than 1 μηη in the longest direction, preferably less than 750 nm, more preferably less than 500 nm in the longest direction, such as in the range 50-1000 nm, preferably 100-750 nm.
  18. The process as claimed in any of claims 13-17, wherein the Sr-ferrite starting material is selected from a low grade Sr-ferrite, high grade Sr-ferrite and recycled Sr-ferrite, or blends of two or more thereof.
  19. The process as claimed in any of claims 13-18, wherein the mixture of Sr- ferrite starting material and iron oxide used in step iii) comprises an amount of Sr- ferrite prior to milling of 85-99.9 wt%, preferably 90-99.5 wt%, preferably 92-99 wt%, preferably 93-97 wt%, based on the total weight of the mixture of Sr-ferrite starting material and Fe<2>0<3>.
  20. The process as claimed in any of claims 13-19, wherein the mixture of Sr- ferrite starting material and iron oxide used in step iii) comprises an amount of iron oxide prior to milling of 0.1 -15 wt%, preferably 0.5-10 wt%, preferably 1 -8 wt%, preferably 3-7 wt%, based on the total weight of the mixture of Sr-ferrite starting material and iron oxide.
  21. The process as claimed in any of claims 13-20, wherein in step iv) the heating is carried out at a temperature of 500-1500 °C, preferably 800-1200 °C, more preferably 900-1 100 °C.
  22. The process as claimed in any of claims 13-21 , wherein in step iv) the heating is carried out for 15 min - 4 hours, such as 30 min - 2 hours, e.g.
  23. hour.
  24. The process as claimed in any of claims 13-22, wherein the iron oxide is Fe<2>0<3>.
  25. The process as claimed in any of claims 13-23, wherein the iron oxide particles prior to milling in step iii) have a diameter of less than 250 nm, such as less than 100 nm, less than 75 nm or less than 50 nm, e.g. in the range 10-250 nm, 15-100 nm, 20-75 nm or 25-50 nm.
  26. The process as claimed in any of claims 13-24, wherein the milling is performed with less than 1 wt% processing control agent (PCA) such as liquid PCA (e.g. water and/or toluene) or solid PCA (stearic acid); preferably the milling in step i) is performed in the absence of a processing control agent (PCA) such as liquid PCA (e.g. water and/or toluene) or solid PCA (stearic acid).
  27. The process as claimed in any of claims 13-25, wherein the material milled in step iii) comprises at least 90 wt% of the mixture of a Sr-ferrite starting material and iron oxide, e.g. at least 95 wt%, 99 wt% or 99.9 wt% of the mixture of a Sr- ferrite starting material and iron oxide.
  28. A two-phase ferrite powder comprising a) Sr-ferrite as a first phase b) an iron oxide as a second phase.
  29. The two-phase ferrite powder as claimed in claim 27, wherein the iron oxide is Fe<2>0<3>.
  30. The two-phase ferrite powder as claimed in claim 27 or 28, having a coercivity of greater than 1 .5 kOe, more preferably greater than 4.5 kOe.
  31. The two-phase ferrite powder as claimed in any of claims 27-29, having a coercivity of greater than 5.0 kOe.
  32. The two-phase ferrite powder as claimed in of claims 27-30, wherein the Sr- ferrite phase is present as the major phase and the iron oxide is present as the minor phase.
  33. The two-phase ferrite powder as claimed in of claims 27-31 , wherein the iron oxide is present in an amount of 0.1 -15 wt%, preferably 0.5-10 wt%, preferably 1 -8 wt%, preferably 3-7 wt%, based on the total weight of the two-phase ferrite powder.
  34. The two-phase ferrite powder as claimed in of claims 27-32, wherein the Sr- ferrite is present in an amount of 85-99.9 wt%, preferably 90-99.5 wt%, preferably 92-99 wt%, preferably 93-97 wt%, based on the total weight of the two-phase ferrite powder.
  35. A two-phase ferrite powder as claimed in any of claims 27-33 formed or formable by the process of any of claims 1 -12.
  36. A two-phase ferrite powder as claimed in any of claims 27-33 formed or formable by the process of claims 13-26.
  37. A process as claimed in any of claims 1 -26, wherein the two-phase ferrite powder is as claimed in any of claims 27-35.
  38. A use of the two-phase ferrite powder as claimed in claims 27-35 as a permanent magnet.
  39. An electric motor comprising a magnet formed from the two-phase ferrite powder as claimed in claims 27-35.
  40. A method of forming a permanent magnet comprising exposing the two- phase ferrite powder of claims 27-35 to a magnetic field.
Inventores
  • REAL, Alberto Bollero
  • DELEDDA, Stefano
  • CAMARERO de DIEGO, Julio
  • GUZIK, Matylda
  • RODRÍGUEZ, Javier Rial
Solicitantes
  • Institutt for Energiteknikk
  • Fundación IMDEA Nanociencia
Clasificación IPC

C01G 49/ 00 A I, C01G 49/ 02 A I, C01G 49/ 06 A I, C01G 49/ 08 A I, C04B 35/ 26 A I, C04B 35/ 626 A I, H01F 1/ 00 A I, H01F 1/ 01 A I, H01F 1/ 032 A I, H01F 1/ 03 A I, H01F 1/ 10 A I, H01F 1/ 34 A I, H01F 1/ 36 A I

Nº de publicación

WO.2018211121.A1

Fecha de publicación

22 de noviembre de 2018

Nº de solicitud

2018063222

Fecha de presentación

18 de mayo de 2018

Estado legal
docdbfechacodigodescripcion
WO.2018211121.A12020-08-05122EP: PCT APPLICATION NON-ENTRY IN EUROPEAN PHASE
WO.2018211121.A12019-11-19NENPNON-ENTRY INTO THE NATIONAL PHASE
WO.2018211121.A12019-01-02121EP: THE EPO HAS BEEN INFORMED BY WIPO THAT EP WAS DESIGNATED IN THIS APPLICATION
Patentes relacionadas