Procedure for obtaining fibres and porous sheets of indium oxide alloyed with tin oxide using thermal evaporation, notably for electron gun bombardment, consisting in performing an electron bombardment with an energy level of up to 10 KeV, at a deposition speed of 35A/min.,evaporation being carried out using a sintered wafer comprising 87% In2O3 and 13% SnO2 weight, performed at glass substrate temperatures (Ts) of 120 degrees C to 400 degrees C at a base pressure of <10-<7> Torr and 2x10-<6>-10-<5> Torr residual. The films obtained have a thickness of several microns, are highly conductive, with random and arborescent growth fibres, it being observed that as Ts increases, so does the size of the fibre, its crystallinity, adherence, conductivity, surface Sn concentration and oxygen deficiency, the resulting deposit being resistant to air heat treatments up to 450 degrees C and usable as an electrochemical sensor or support for elements used as catalyses.< IMAGE >The method is new. The method comprises bombardment with electrons of energy up to 10 KeV, with deposit velocity 35 AA/second to cause evaporation of tablet composed of 87 wt.% of In2O3 and 13 wt.% of SnO2, at temperature of glass substrate (Ts) 120-400[deg]C, base pressure 1->7> Torr and residual pressure 2 X 10->6> - 10->5> Torr. Obtained films have various thicknesses, high conductivity, and chaotic and arborescent fiber growth. Increase of substrate temperature Ts results in increased size of fibers, crystallinity, adherence, conductivity, surface concentration of Sn and oxygen deficiency. Obtained deposit is resistant to thermal treatment in presence of air up to 450[deg]C.
C01G 15/ 00 A I, C01G 19/ 02 A I, C04B 35/ 00 A I, C22C 13/ 00 A I, C22C 28/ 00 A I, C23C 14/ 34 A I
ES.2147487.A1
1 de septiembre de 2000
ES19970001004
9 de mayo de 1997
| docdb | fecha | codigo | descripcion |
|---|---|---|---|
| ES.2147487.A1 | 2017-08-25 | FD2A | ANNOUNCEMENT OF LAPSE IN SPAIN |
| ES.2147487.A1 | 2000-09-01 | EC2A | SEARCH REPORT PUBLISHED |